MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Radici Radilon® Aestus T2 RV350W 333 BK Polyphthalamide
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 40% Glass Fiber Reinforced

Material Notes: PPA injection molding grade 35% glass fiber reinforced high melting point. Heat stabilized. Black color.

Suitable for parts requiring high stiffness and strength. Intended to work at high temperatures.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³DAM; ISO 1183
Water Absorption 0.20 %
@Thickness 2.00 mm,
Time 86400 sec
0.20 %
@Thickness 0.0787 in,
Time 24.0 hour
Immersion @ 23°C; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 160 MPa23200 psi5mm / min. Conditioned; ISO 527-2/1A
 185 MPa26800 psi5mm / min. DAM; ISO 527-2/1A
Elongation at Break 1.9 %1.9 %5 mm / min. DAM; ISO 527-2/1A
 2.2 %2.2 %5 mm / min. Conditioned; ISO 527-2/1A
Tensile Modulus 10.9 GPa1580 ksi1mm / min. Conditioned; ISO 527-2/1A
 12.15 GPa1762 ksi1mm / min. DAM; ISO 527-2/1A
Flexural Strength 285 MPa41300 psi2mm / min. DAM; ISO 178
Flexural Modulus 10.5 GPa1520 ksi2mm / min. DAM; ISO 178
Charpy Impact Unnotched  4.60 J/cm²
@Temperature -30.0 °C
21.9 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 5.50 J/cm²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  1.15 J/cm²
@Temperature -30.0 °C
5.47 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1e/A
 1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmDAM; 500V.; IEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmDAM; 500V.; IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 18.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
10.0 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 73.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
40.6 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Melting Point 310 °C590 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 280 °C536 °FISO 75/2Af
Flammability, UL94 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 320 - 340 °C608 - 644 °FInjection Molding
Mold Temperature 100 - 120 °C212 - 248 °F
 
Descriptive Properties
Injection Molding Injection SpeedMedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADI6937 / 293442

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.