MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ganpati Exim BP93 Citric Acid Anhydrous
Categories: Other Engineering Material

Material Notes: Citric acid is a weak organic acid. It is a natural preservative and is also used to add an acidic, or sour, taste to foods and soft drinks. In biochemistry, it is important as an intermediate in the citric acid cycle and therefore occurs in the metabolism of almost all living things. It also serves as an environmentally benign cleaning agent and acts as an antioxidant. Citric acid exists in a variety of fruits and vegetables, most notably citrus fruits. Lemons and limes have particularly high concentrations of the acid; it can comprise as much as 8% of the dry weight of these fruits (1.44 and 1.38 grams per ounce of the juices, respectively).

Applications: Citric Acid is mainly used as acidulant, flavoring agent, preservative and antistaling agent in food and beverage industry. Moreover, it is also used as antioxidant, plasticizer and detergent in chemical, cosmetics and cleaning industries.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Ash <= 0.10 %<= 0.10 %Sulphated
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 1.0 %<= 1.0 %
 
Descriptive Properties
AppearanceColorless Crystals or Crystal Powders
Content<1 ppmArsenic
 <10 ppmHeavy Metals (as Pb)
 <150 ppmSulphate
 <200 ppmCalcium
 <350 ppmOxalate
 <50 ppmChloride
 <50 ppmIron
 99.5-101%Content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGANPATI101 / 317385

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.