MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Master Bond X5G One Component, Graphite Filled Elastomeric Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive, Flexible; Epoxy, Electrically Conductive

Material Notes: Key Features:
  • One part, no mix system
  • Cures at room or elevated temperatures
  • Fast curing
  • Good electrical conductivity
Master Bond X5G is an easy to use, solvent based elastomeric system with reliable electrical conductivity. X5G has a paste-like consistency and when used as an adhesive, it is simply applied in a thin layer to one of the substrates. The surfaces are then coupled, fixtured and the product is allowed to cure. X5G can also be applied in the same manner for coating. Curing takes place by the evaporation of the solvent. RoHS Compliant.

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/cc
Water Absorption <= 0.50 %
@Time 86400 sec
<= 0.50 %
@Time 24.0 hour
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.0 - 10 ohm-cm
@Temperature 23.9 °C
5.0 - 10 ohm-cm
@Temperature 75.0 °F
Surface Resistance 5.0 - 40 ohm
@Temperature 75.0 °C
5.0 - 40 ohm
@Temperature 167 °F
Shielding Effectiveness 40 - 50 dB
@Frequency 1000 - 1.00e+9 Hz
40 - 50 dB
@Frequency 1000 - 1.00e+9 Hz
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.720 - 1.01 W/m-K5.00 - 7.01 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 90.0 min
@Temperature 65.6 °C
1.00 - 1.50 hour
@Temperature 150 °F
option 1
 480 - 720 min
@Temperature 23.9 °C
8.00 - 12.0 hour
@Temperature 75.0 °F
option 2
Shelf Life 3.00 Month
@Temperature 23.9 °C
3.00 Month
@Temperature 75.0 °F
in original, unopened containers
 
Descriptive Properties
ColorBlack
Viscositypaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy
Master Bond EP75-1 Graphite Filled Electrically Conductive Epoxy System
Parker Chomerics CHO-SEAL® S6600 Conductive Elastomer
Parker Chomerics CHO-SEAL® 6307 Conductive Elastomer
Overview of materials for Epoxy, Electrically Conductive

PMASTM982 / 187000

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.