MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® SP-14077 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene SP-14077 is a general purpose thermoplastic elastomer designed for a variety of consumer applications, including sports and recreating applications, requiring a soft, rubber-like feel. Monprene SP-14077 is a medium hardness, low density grade that exhibits medium flow characteristics and is suited for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Colorability; Good Flexibility; Good Moldability; Good Processability; Good Toughness; Medium Flow; Low Density; Low Specific Gravity; Medium Hardness; Resilient; Weather Resistant; Without Fillers

Uses: Consumer Applications; Flexible Grips; Gaskets; Grommets; Handles; Plugs; Rubber Replacement; Soft Touch Applications; Sporting Goods; Swimming Pools

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccASTM D792
Melt Flow 17 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75
@Time 5.00 sec
Injection Molded; ASTM D2240
 77
@Time 1.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 1160 psiDie C, 20 in/min, Flow; ASTM D412
 1370 psiDie C, 20 in/min, Across Flow; ASTM D412
Tensile Stress at Strain 444 psi
@Strain 100 %
Die C, 20 in/min, Across Flow; ASTM D412
 642 psi
@Strain 100 %
Die C, 20 in/min, Flow; ASTM D412
 650 psi
@Strain 300 %
Die C, 20 in/min, Across Flow; ASTM D412
 871 psi
@Strain 300 %
Die C, 20 in/min, Flow; ASTM D412
Elongation at Break 500 %Die C, 20 in/min, Flow; ASTM D412
 670 %Die C, 20 in/min, Across Flow; ASTM D412
Tear Strength 228 pliDie C, 20 in/min, Flow; ASTM D624
 252 pliDie C, 20 in/min, Across Flow; ASTM D624
Compression Set 23 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ASTM D395B
 92 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ASTM D395B
 
Processing PropertiesOriginal ValueComments
Processing Temperature 390 - 480 °FMelt, Injection
Rear Barrel Temperature 360 - 450 °FInjection
Middle Barrel Temperature 370 - 460 °FInjection
Front Barrel Temperature 380 - 470 °FInjection
Nozzle Temperature 390 - 480 °FInjection
Zone 1 360 - 450 °FExtrusion
Zone 2 370 - 460 °FExtrusion
Zone 3 380 - 470 °FExtrusion
Zone 4 380 - 470 °FExtrusion
Zone 5 390 - 480 °FExtrusion
Die Temperature 390 - 480 °FExtrusion
Mold Temperature 95.0 - 120 °FInjection
Injection Pressure 200 - 800 psiInjection
Back Pressure 25.0 - 100 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Monprene® SP-14966 Thermoplastic Elastomer
Teknor Apex Monprene® SP-16920 XRD2 Thermoplastic Elastomer
Teknor Apex Monprene® SP-14986 XRD1 Thermoplastic Elastomer
Axiall CL-6380, CL-6380J Rigid PVC, Molding
A. Schulman Diamond Centrex® 825 Sheet Extrusion Grade

PTEKNQ0957 / 237448

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.