MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Elastosil® R 562/80 Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: ELASTOSIL® R 562/80 is a peroxide crosslinking HCR silicone for the manufacture of silicone-insulated cables and wires.

Properties: The mechanical properties refer to crosslinker C6. The compound is colored anthracite. Addition of 2.2% ELASTOSIL® AUX SB-2 increases the LOI to 32 %.

Special features:

  • good mechanical and electrical properties
  • high dielectric strength
  • high volume resistivity
  • good heat resistance
  • good rheological properties
  • very good oil and fuel resistance
  • combustion products of low toxicity and corrosivity and low smoke density
Application: Cable insulations with high hardness in ignition cables, measuring equipment, components under high voltage.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³DIN 53479
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7878DIN 53505
Tensile Strength at Break 8.80 MPa1280 psiDIN 53504 S1
Elongation at Break 300 %300 %DIN 53504 S1
Tear Strength 20.0 kN/m114 pliASTM D624 B
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmDIN IEC 93
Dielectric Constant 3.03.0DIN VDE 0303
Dielectric Strength 26.0 kV/mm660 kV/inDIN IEC 243-1
Dissipation Factor 0.000200.00020DIN VDE 0303
 
Descriptive Properties
Appearanceblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9221 / 204750

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.