Capabilities- Gauge: .001” to .004” (28 to 101µm)
- Width: .2” to 80” (50.8 to 2032mm)
- Core size: 3” and 6” standard cores, 8” available
- Roll O.D.: various configurations available
- Custom colors and tints available
- 3 strategic manufacturing locations
Properties - Low gloss formula for better optical character recognition
- Low dust for higher production rates
- Engineered orientation for optimal tear properties
- Specially formulated to reduce scratching
- Excellent stiffness for improved processability
Information provided by Alcoa Kama Co. |