MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Nouryon Trigonox A-W70 Acrylics tert-Butyl hydroperoxide, 70% solution in water
Categories: Other Engineering Material

Material Notes: Trigonox A-W70 is an initiator (70% active ingredient in water) for (co)polymerization of (meth)acrylates.

CAS number: 75-91-2

EINECS/ELINCS No: 200-915-7

Applications: Polymer production: Trigonox A-W70 can be used as an initiator in bulk, aqueous solution and emulsion polymerization of styrene, acrylates and methacrylates. The polymerization can be initiated by radicals generated by the thermal decomposition of Trigonox A-W70 above 110°C or through a redox mechanism at low temperatures. Effective organic reducing agents are ascorbic acid and sodium formaldehyde sulfoxylate, possibly combined with heavy metal compounds such as cobalt or iron salts. Thermoset: Trigonox A-W70 may be used as an initiator for the room temperature cure of promoted unsaturated polyester and vinyl ester resins, and elevated cure of non-promoted resins.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc
@Temperature 25.0 °C
0.0338 lb/in³
@Temperature 77.0 °F
Half-life  0.100
@Temperature 207 °C
0.100
@Temperature 405 °F
[hr]
 1.00
@Temperature 185 °C
1.00
@Temperature 365 °F
[hr]
 10.0
@Temperature 164 °C
10.0
@Temperature 327 °F
[hr]
Viscosity 4.1 cP
@Temperature 20.0 °C
4.1 cP
@Temperature 68.0 °F
Molecular Weight 90.1 g/mol90.1 g/mol
Storage Temperature 0.000 - 35.0 °C32.0 - 95.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear colorless liquid
Assay69.0-71.0 %
Color<20 Pt-Co / APHA
Content12.25-12.61 %Active oxygen
Content (%)17.76Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1150 / 286673

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.