MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wellman Wellamid® GSF25/15-66 22L-N 40% Glass Sphere/Fiber Reinforced Nylon 66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description: Glass Sphere/Fiber Reinforced Nylon 66

Information provided by Wellman.

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ISO 1183-87
Filler Content 40 %40 %
Linear Mold Shrinkage, Flow 0.0050 - 0.0090 cm/cm0.0050 - 0.0090 in/inISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.012 - 0.016 cm/cm0.012 - 0.016 in/inISO DIS 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 115 MPa16700 psiISO 527-93
Elongation at Break 2.5 %2.5 %ISO 527-93
Flexural Strength 180 MPa26100 psiISO 178-93
Flexural Modulus 7.50 GPa1090 ksiISO 178-93
Izod Impact, Notched (ISO) 3.00 kJ/m²1.43 ft-lb/in²ISO 180-93
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FISO 75-93
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 282 - 304 °C540 - 580 °F
Middle Barrel Temperature 271 - 288 °C520 - 550 °F
Front Barrel Temperature 260 - 277 °C500 - 530 °F
Nozzle Temperature 260 - 288 °C500 - 550 °F
Melt Temperature 277 - 304 °C530 - 580 °F
Mold Temperature 71.1 - 93.3 °C160 - 200 °F
Drying Temperature 79.4 °C175 °FOpened bags and gaylord boxes
Dry Time 2 - 4 hour2 - 4 hourOpened bags and gaylord boxes
Moisture Content 0.050 - 0.20 %0.050 - 0.20 %During molding to prevent hydrolytic degradation
 <= 0.20 %<= 0.20 %In shipping bags, ready to mold
Injection Pressure 34.5 - 138 MPa5000 - 20000 psi
Back Pressure 0.345 MPa50.0 psi
Screw Speed 60 - 120 rpm60 - 120 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEL671 / 72387

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.