MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Covestro Makrolon® 15 sheet Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Extended abrasion and UV resistance Makrolon® 15 sheet is a polycarbonate product that offers excellent impact resistance in high risk areas, weathering life, and optical quality. It provides a clear aesthetic advantage over wire glass and metal screens for security glazing. Makrolon 15 protects against vandalism, forced entry attempts or attacks, and accidental impacts to minimize the risk of theft and glass replacement in damageprone areas. Advanced manufacturing technology has resulted in high optical quality with minimal distortion in clear and standard glazing tints. The abrasion resistant coating, applied to both sides, provides up to twice the life of prior polycarbonate sheet products. Makrolon 15 sheet has a fifteen (15) year Limited Product Warranty against breakage, yellowing, and loss of light transmission.

Applications: Educational, psychiatric and medical facilities, retail and government buildings, and transportation centers at risk from breakage and vandalism

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 65.5 MPaASTM D638
Tensile Modulus 2340 MPaASTM D638
Flexural Strength 93.1 MPaASTM D790
Izod Impact, Notched 16.0 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched 60.0 ft-lb/in
@Thickness 3.17 mm
no failure; ASTM D256
Impact Test >= 47.0 ft-lb
@Thickness 3.17 mm
ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 37.5 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 142 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 86 %
@Thickness 3.00 mm
ASTM D1003
 
Descriptive Properties
Chemical ResistanceAcetone>24 Hrs
 Ammonia (10% concentration)>24 Hrs
 Antifreeze (50/50)>24 Hrs
 Benzene>24 Hrs
 Bleach (Clorox concentrated)>24 Hrs
 Chloroform>24 Hrs
 Denatured Alcohol>24 Hrs
 Di (2-ethylhexyl) phthalate>24 Hrs
 Diesel Oil>24 Hrs
 Hydrochloric Acid (20%)>24 Hrs
 Isopropyl Alcohol (IPA)>24 Hrs
 Kerosene>24 Hrs
 Methyl Alcohol>24 Hrs
 Methyl Butyl Ketone>24 Hrs
 Methyl Ethyl Ketone>24 Hrs
 Methylene Chloride>24 Hrs
 Naphthalene, 1-bromo->24 Hrs
 Nitric Acid (20%)>24 Hrs
 Potassium Hydroxide - Lye (10%)>24 Hrs
 Sodium Hydroxide (10%)>24 Hrs
 Sulfuric Acid (20%)>24 Hrs
 Toluene>24 Hrs
 Turpentine>24 Hrs
 Unleaded Gasoline (87 Octane)>24 Hrs
 Vinegar>24 Hrs
 Xylene>24 Hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® 1095 Polycarbonate, 15% Glass Filled
Covestro Makrolon® 1260 Polycarbonate, Impact Grade
Covestro Makrolon® 1248 Polycarbonate, Impact Grade
Covestro Makrolon® 1248 MAS068 Polycarbonate
Zircar Zirconia ZYBF-1 Zirconia Bulk Fiber Insulation

PCOVEST0866 / 202649

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.