MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC SABIC® LLDPE 218BJ PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: SABIC® LLDPE 218BJ is a butene linear low density polyethylene resin with an additive package typically designed for a broader range of food applications (TNPP free). The good thermal stability allows to use the resin in critical extrusion processing conditions. Films produced from SABIC® LLDPE 218BJ have better draw-down ability compared to lower MFR LLDPE resins. This product is not intended for and must not be used in any pharmaceutical/medical applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 48ISO 868
Tensile Strength at Break 17.0 MPaASTM D638
Tensile Strength, Yield 12.0 MPaASTM D638
Elongation at Break 790 %ASTM D638
Elongation at Yield 16 %ASTM D638
Flexural Modulus, 1% Secant 254 MPaASTM D790
Puncture Energy 2.20 JProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D5748-95
Tear Strength 185 kN/mTD; Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ISO 6383-2
Peel Strength 0.0500 kN/m200% pre-stretch; ASTM D5458-95
 0.0600 kN/m0% pre-stretch; ASTM D5458-95
Dart Drop Total Energy 28.0 J/cmProperties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ISO 7765-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+15 ohm-cmASTM D257
Dielectric Constant 2.17
@Frequency 60 Hz
ASTM D150
Dielectric Strength 55.0 kV/mm500 V/sec; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Melting Point 122 °CSABIC method
 122 °CSABIC method
Vicat Softening Point 96.0 °Cat 10 N (VST/A); ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 1.2 %
@Thickness 0.0300 mm
2.5 BUR using 100% 218BJ.; ASTM D1003
Gloss 92 %45°; Properties have been measured by producing 30 µm film with 2.5 BUR using 100% 218BJ.; ASTM D2457
 
Descriptive Properties
Elastic recovery52.6 %ASTM D5459-95; 30 µm film with 2.5 BUR using 100% 218BJ.
Retention force at 60 sec0.97 kg
Stress retention80 %ASTM D5459-95; 30 µm film with 2.5 BUR using 100% 218BJ.
Ultimate pre-stretch level310 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11046 / 244513

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.