MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

SCG Chemicals EL-Lene™ H5615F High Density Polyethylene Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Key Characteristics:
  • High speed processing
  • High tensile strength
  • High dart impact
  • Low gel content
  • Good moisture barrier

Recommended Applications: Ultra thin film (<10 micron) for shopping bag, T-shirt bag, garbage bag, liner bag

Information provided by SCG Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.956 g/cc0.956 g/ccASTM D1505
Environmental Stress Crack Resistance >= 1000 hour
@Temperature 50.0 °C
>= 1000 hour
@Temperature 122 °F
F50, 25% Igepal; ASTM D1693
Thickness 12.0 microns0.472 mil
Melt Flow 0.15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.15 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, TD 30.0 MPa4350 psiASTM D882
Film Elongation at Break, MD 160 %160 %ASTM D882
Film Elongation at Break, TD 360 %360 %ASTM D882
Secant Modulus, MD 0.950 GPa138 ksiASTM D882
Secant Modulus, TD 0.980 GPa142 ksiASTM D882
Elmendorf Tear Strength MD 3.0 g3.0 gASTM D1922
Elmendorf Tear Strength TD 118 g118 gASTM D1922
Elmendorf Tear Strength, MD 0.250 g/micron6.35 g/milASTM D1922
Elmendorf Tear Strength, TD 9.83 g/micron250 g/milASTM D1922
Dart Drop 8.90 g/micron226 g/milASTM D1709
Dart Drop Test 107 g0.236 lbASTM D1709
Film Tensile Strength at Break, MD 45.0 MPa6530 psiASTM D882
Film Tensile Strength at Break, TD 28.0 MPa4060 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FASTM D2117
Vicat Softening Point 123 °C253 °FASTM D1525
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SCG Chemicals EL-Lene™ H5604F High Density Polyethylene Film
Braskem H502-25RG Extrusion Polypropylene
LyondellBasell Petrothene® NA204000 Low Density Polyethylene
Lotte Chemical Titan TITANLENE® LDC800YY Low density polyethylene resin
Huntsman Rexell® L3102 Blown Film Extrusion LLDPE

PSCGC903 / 120657

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.