Electrically conductive two component silicone rubber grades for extrusion of profiles and cable components in hot air. Properties: The materials are black due to their conductivity. Special features: - good mechanical and electrical properties
- high conductivity
- low volume resistivity
- good heat resistance
- good rheological properties
- combustion products of low toxicity and corrosivity and low smoke density
- none cross-linking agent crack products
- flame retardant
Application: electrically conductive profiles, EMI-gaskets, ignition cables (core), band electrodesInformation provided by Wacker Chemie AG. |