MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Kao-Tex­™ Textile 2000 Ceramic Fiber Cloth Sintered Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Kao-Tex Textile 2000 Cloths are made from alumina-silica ceramic fibers that are reinforced with an organic carrier fiber for added strength and stability, making them an excellent choice for industrial applications. The nature of the engineered yarns and weave types, provide excellent strength, resulting in a physically resilient material well suited to high temperature industrial applications.

Applications:

  • Welding, Fire, Oven and Drop curtains
  • Stress Relieving blankets
  • Fire and Heat barriers
  • Removable Insulation
  • Lagging
  • Fabric Expansion joints
  • Gasketing and Sealing
  • Gloves and Mittens

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air <= 1093 °CContinuous Use
 
Descriptive Properties
Colorgray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceramic Fiber Board S Board Ceramic Fibre Board
Thermal Ceramics Alfibond 2100 Shapes
Morgan Advanced Ceramics Kaowool Ceramic Felt 1260 Thermal Ceramic
Morgan Advanced Ceramics Ceramic Fiber Ropes Twisted Ceramic Fiber
Morgan Advanced Ceramics Ceramic Fiber Blankets Cerawool Blanket

CMORF6496 / 203280

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.