MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kolon Kopa® KN133HB55 Nylon 6 Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: KOPA is widely used in the automobile and industrial parts.

General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent chemical resistance, Wide usage temperature, Good impact absorbing characteristics.

Information provided by US distributor, API-Kolon.

Key Words: Polyamide 6; PA6; PA 6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.63 g/cc0.0589 lb/in³DIN 53479; ASTM D792
Water Absorption 0.70 %0.70 %DIN 53475; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120DIN 53505; ASTM D785
Tensile Strength, Ultimate 177 MPa25700 psiDIN 53455; ASTM D638
Elongation at Break 4.0 %4.0 %DIN 53455; ASTM D638
Flexural Yield Strength 246 MPa35700 psiDIN 53452; ASTM D790
Flexural Modulus 11.8 GPa1710 ksiDIN 53452; ASTM D790
Izod Impact, Notched 0.690 J/cm1.29 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 22.0 kV/mm559 kV/inASTM D149/DIN 53481
Arc Resistance 136 sec136 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 40.0 µm/m-°C
@Temperature 20.0 °C
22.2 µin/in-°F
@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 220 °C428 °FDIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FDIN 53461; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 180 °C356 °FDIN 53461; ASTM D648
Flammability, UL94 HBHB

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLAKG1 / 49842

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.