MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dow ELITE™ 5220G Enhanced Polyethylene Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes:
  • High impact and puncture resistance
  • Excellent on-pallet load elongation for higher yields on regular loads
  • Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.915 g/cc0.0331 lb/in³ASTM D792
Thickness 20.3 microns0.800 mil
Melt Flow 3.5 g/10 min3.5 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 8.96 MPa1300 psiASTM D882
Film Tensile Strength at Yield, TD 8.41 MPa1220 psiASTM D882
Film Elongation at Break, MD 450 %450 %ASTM D882
Film Elongation at Break, TD 650 %650 %ASTM D882
Elongation, Ultimate 300 %300 %on-pallet testing, by LANTECH SHS Tester; Dow Method
Impact 1010[lbf]; Puncture Resistance Force; Dow Method
 4949[N]; Puncture at 250% pre-stretch; on-pallet testing determined by LANTECH SHS Tester; Dow Method
 323323[ft-lbf/in3]; Puncture Resistance; Dow Method
Puncture Energy 4.07 J3.00 ft-lbDow Method
Elmendorf Tear Strength MD 390 g390 gASTM D1922
Elmendorf Tear Strength TD 600 g600 gASTM D1922
Elmendorf Tear Strength, MD 19.19 g/micron487.5 g/milASTM D1922
Elmendorf Tear Strength, TD 29.5 g/micron750 g/milASTM D1922
Dart Drop Test 630 g1.39 lbMethod B; ASTM D1709
Film Tensile Strength at Break, MD 40.0 MPa5800 psiASTM D882
Film Tensile Strength at Break, TD 35.9 MPa5200 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 123 °C253 °FDow Method (DSC)
Vicat Softening Point 99.0 °C210 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 0.60 %0.60 %ASTM D1003
Gloss 96 %96 %45°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow ELITE™ 5230G Enhanced Polyethylene Resin
Dow ELITE™ 5400G Enhanced Polyethylene Resin
Silberline Tufflake® 3620
Dow ELITE™ 5100G Enhanced Polyethylene Resin
Dow ELITE™ 5110G Enhanced Polyethylene Resin

PDOW1324 / 30542

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.