MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro MAKROFOL® LM 296 1-2 760125 Polycarbonate Films
Categories: Polymer; Film; Thermoplastic; Polycarbonate (PC)

Material Notes: Characterization: Makrofol LM 296 1-2 760125 is an extruded film based on Makrolon® polycarbonate.

Properties / Applications: Makrofol LM 296 1-2 760125 is a gray colored extruded film based on Makrolon polycarbonate from Covestro. The film is tailor made for use in Black Panel Technology. It comprises a precisely defined light transmission within minimum tolerances at defined wave lengths, as well as a defined film surface. Typical applications are instrument panels and touch panels. Makrofol LM 296 1-2 760125 is available in a standard thicknesses of 0.020" (500 microns). Other thicknesses available on request. The surface structure of Makrofol LM 296 1-2 760125 is one side gloss, and one side very fine matte (1-2). As with any product, use of Makrofol LM 296 1-2 760125 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccISO 1183, Method C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPaISO 527-1,-3
Elongation at Break 100 %ISO 527-1,-3
Tensile Modulus 2100 MPaISO 527-1,-3
 
Optical PropertiesOriginal ValueComments
Gloss 25 %2-side; ISO 2813
 >= 98 %1-side; ISO 2813
Transmission, Visible 25 %ISO 13468-2 following DIN 5036

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrofol® BL 2-4 820816 Polycarbonate
Covestro Makrofol® BL 6-2 820803 Polycarbonate
Covestro Makrofol® BL 6-2 820802 Polycarbonate
Covestro MAKROFOL® LM 296 1-2 760225 Polycarbonate Films
Covestro Makrofol® ID 6-2 laserable Polycarbonate

PCOVEST0807 / 202590

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.