MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Resin Technology Group KONA 870FT-FR Fire Retardant Epoxy Casting System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Mix ratio 100 to 4 by weight.

KONA 870 FTFR with HARDENER #9 is a versatile epoxy casting system that exhibits unusually high thermal conductivity and low thermal expansion. It is recommended for electronic/electrical casting and encapsulating applications that require a unique combination of excellent wetting, flow, good thermal expansion coefficient, thermal shock resistance, high heat transfer capabilities and outstanding electrical properties. Fully cured KONA 870 FTFR with HARDENER #9 is highly resistant to water, weather, gases and vapors, petroleum lubricants and fuels, and many mild acids and alkalis. This system is room temperature curing with a 45 minute pot life (1 pound mass), has a high viscosity with good handling properties, and is tough and rigid at all temperatures to 300°F.

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.30 g/cc
Viscosity 90000 cP
@Temperature 25.0 °C
Mixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 91
Tensile Strength at Break 7700 psi
Compressive Strength 15200 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 536 V/mil
Dissipation Factor 0.0020
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 151 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 150 °C
 24.0 hour
@Temperature 25.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Resin Technology Group KONA 877 Low Viscosity, Low Shrinkage, Vacuum Grade Casting Resin
Resin Technology Group TIGA 108 Room Temperature Curing Epoxy Adhesive
Resin Technology Group 451 Oxy-Bond™ Electrically Conductive Epoxy Adhesive
Resin Technology Group KONA 871 Low Cost Epoxy Resin
Resin Technology Group 405 Oxy-Bond™ Electrically Conductive Epoxy Adhesive

PRESINT640 / 65524

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.