MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Von Roll Isola IMI Varnish 74036 Solventless Epoxy Varnish for Electrical Insulation
Categories: Polymer; Thermoset; Epoxy; Solventless Epoxy Varnish, Electrical Insulation

Material Notes: Data provided by Von Roll Isola USA.

IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >93°C. Usage Notes: Excellent moisture and chemical resistance.

Key Words: Von Roll Isola USA; Insulating Materials Incorporated
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/cc
Viscosity 3200 cP
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 87.0 kV/mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 100 °CSuggested baking time at this temperature is 0.25 hr.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Von Roll Isola IMI Varnish 74035 Solventless Epoxy Varnish for Electrical Insulation
Von Roll Isola IMI Varnish 74030 Solventless Epoxy Varnish for Electrical Insulation
Von Roll Isola IMI Varnish 74011 Solventless Epoxy Varnish for Electrical Insulation
Von Roll Isola IMI Varnish 74010A Epoxy Varnish for Electrical Insulation
Von Roll Isola IMI Varnish 74001 Epoxy Varnish for Electrical Insulation

PISO15 / 48418

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.