MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
TSRC T-BLEND® 1003-35C TPR/TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: T-BLEND® is a series of thermoplastic rubber compound materials produced by TSRC CORPORATION. With the advantages of weather durable, rebound resilience, compression and bending properties, T-BLEND® 1003-35C may be applied to a variety of unique products by injection molding machine. T-BLEND® 1003-35C is a palletized elastomer compound based on styrenic block copolymer. T-BLEND® 1003-35C thermoplastic elastomer compound is recyclable including wastes from gate and runner.

Information provided by TSRC Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccASTM D792
Linear Mold Shrinkage 0.015 - 0.025 in/in
Melt Flow 43 g/10 min
@Load 2.16 kg,
Temperature 180 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35ASTM D2240
Tensile Strength 51.0 kg(f)/cm²Type3, specimen; ASTM D412
Elongation at Break 1124 %500 mm/min; ASTM D412
300% Modulus 19.0 kg(f)/cm²500mm/min; ASTM D412
Rebound >= 60 %ASTM D2632
Tear Strength 22.0 kg(f)/cmC Die; ASTM D624
 
Thermal PropertiesOriginal ValueComments
Shrinkage <= 2.0 %
@Temperature 50.0 °C,
Time 2410 sec
 
Processing PropertiesOriginal ValueComments
Feed Temperature 160 °C
Rear Barrel Temperature 170 °C
Front Barrel Temperature 180 °C
Nozzle Temperature 190 °C
Mold Temperature 30.0 - 40.0 °C
Back Pressure 0.343 - 0.686 MPa
Cycle Time - Injection 25 - 50 sec
 
Descriptive Properties
ColorTranslucent
FormPellets
Light fastness (UV)430W * 253.7 nm, UV light*4 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTSRC044 / 306332

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.