WESTLAKE polyethylene EP413 is a low-density polyethylene recommended for blown or cast film clarity applications. This material has very good optical properties, and is suggested for bakery films , produce bags, and general purpose clarity applications.Application/Uses- General purpose clarity
- Medium duty produce bags
- Bakery bags
- Bags for textile items
FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical |
Very good optical properties |