MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Pyro-Putty™ 1500 High Temperature Ceramic-Metallic Putty, Ceramic Filled
Categories: Ceramic; High Temp Ceramic Resin

Material Notes: Pyro-Putty® High Temperature Pastes are used to seal joints and repair defects in cast aluminum, cast iron, steel and stainless steel. Formulated using the most advanced organic and inorganic-ceramic technologies, these materials resist temperatures to over 2000°F. Applications for Pyro-Putty® are widespread and found typically in the aerospace, automotive, foundry, heat treating, incineration, and power generation industries.

Pyro-Putty® 1500

  • Ceramic Fiber Filled, Organic-Resinous Gasket Seal
  • Seals Boiler Doors & Molten Metal Systems
  • Easy to Apply & Remove, For Uses to 2300°F
Typical Applications:
  • Turbines
  • Boilers
  • Heat Exchangers
  • Compressors
  • Pumps
  • Blowers
  • Piping
  • Ducting
  • Furnaces
  • Ovens
  • Steam Valves
  • Foundry Molds

Vendors: Aremco’s Pyro-Putty high temperature ceramic-metallic pastes seal joints and repair defects in cast aluminum, cast iron, steel and stainless steel to 2300°F (1260°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/cc
Storage Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1260 °C2300 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min1.00 hour1-2 hrs Air Set; 1 hr at 200°F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorGray Brown
FillerCeramic Fiber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon R37292S018 0.018" (0.457 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Substrate
Chosun Refractories 1500 ACE BLANKET Blanket
Sinotek Materials Packing PTFE Braided with Graphite
Rogers Arlon CLTE Microwave Printed Circuit Board Substrate
Rogers Arlon 99790N010 0.010" (0.254 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier

CAREM34 / 575

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.