MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Stratasys® ABS-M30i
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: ABS-M30i is a high strength material well suited for the medical, pharmaceutical and food packaging industries. Parts manufactured with ABS-M30i material are biocompatible (ISO 10993 USP Class VI) and can be gamma or EtO sterilized. When combined with Fortus® 3D Production Systems, ABS-M30i gives you biocompatible Real Parts™ with excellent mechanical properties that are well suited for conceptual modeling, functional prototyping, manufacturing tools, and end-use-parts.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 109.5ASTM D785
Tensile Strength, Yield 36.0 MPaType 1, 0.2"/min, 0.125"; ASTM D638
Elongation at Yield 4 %Type 1, 0.2"/min, 0.125"; ASTM D638
Tensile Modulus 2.400 GPaType 1, 0.2"/min, 0.125"; ASTM D638
Flexural Strength 61 MPaMethod 1, 0.05"/min; ASTM D790
Flexural Modulus 2.300 GPaType 1, 0.2"/min, 0.125"; ASTM D790
Izod Impact, Notched 139 J/mMethod A; ASTM D256
Izod Impact, Unnotched 2.83 J/cmMethod A; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.00e+13 - 1.50e+14 ohm-cmASTM D257
Dielectric Constant 2.7 - 2.9ASTM D150-98
Dielectric Strength 80.0 - 370 V/milMethod A; ASTM D149-09
Dissipation Factor 0.0051 - 0.0053ASTM D150-98
 
Thermal PropertiesOriginal ValueComments
CTE, linear 88.2 µm/m-°C
@Temperature -40.0 - 37.8 °C
ASTM E831
CTE, linear, Transverse to Flow 84.6 µm/m-°C
@Temperature -40.0 - 37.8 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 96.0 °C0.125", unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C0.125", unannealed; ASTM D648
Vicat Softening Point 99.0 °CRate B/50; ASTM D1525
Glass Transition Temp, Tg 108 °C
Flammability, UL94 HB0.06"
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Stratasys® ABS-M30
Stratasys® Ultem 9085 for Rapid Prototyping
Stratasys® PPSF Polyphenylsulfone for 3D Printing
Stratasys® ABSi
Stratasys® PC-ABS

PSTRAT015 / 88888

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.