MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
INEOS Styrolution Absolac® 320 Acrylonitrile Butadiene Styrene (ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Absolac ® 320 is an easy-flow, standard impact, refrigerant injection molding grade suitable for appliances sector. Good chemical resistance, Refrigeration grade, Good flow, Balance mechanical properties. Applications: Refrigerator parts, End cap, Washing machine parts, Water Purifiers

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cmISO 294-4
Melt Flow 16 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110ISO 2039-2
Tensile Strength, Yield 52.0 MPaISO 527
Tensile Modulus 2600 MPaISO 527
Flexural Strength 75.0 MPaISO 178
Flexural Modulus 2700 MPaISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²
@Temperature 23.0 °C
0.25 inch bar, 0.01 notch radius; ISO 180/A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 - 100 µm/m-°CISO 11359
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 98.0 °C
@Load 5.10 kg
B/2 120C/H; ASTM D 1525
 
Optical PropertiesOriginal ValueComments
Gloss 98 %at 60°, specular; ASTM D523

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo Magnum™ 3453 Acrylonitrile Butadiene Styrene (ABS)
LG Chemical TR-558A ABS, Transparent, High Strength
LG Chemical TR300 MABS, Flame Retardant, Transparency
LG Chemical HI100X ABS, High Impact, Semi-Transparency, Flexible
A. Schulman Diamond TR 5000

PSTYR9805 / 216032

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.