MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized; Nylon 66, Unreinforced, Flame Retardant

Material Notes: Polyamide 66 (PA66) based compound. Heat stabilized. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/cc
Linear Mold Shrinkage, Flow 0.0105 - 0.0135 cm/cm
Linear Mold Shrinkage, Transverse 0.0105 - 0.014 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPa
@Temperature 60.0 °C
 70.0 MPa
@Temperature 23.0 °C
Elongation at Break 8.0 %
@Temperature 23.0 °C
 45 %
@Temperature 60.0 °C
 >= 100 %
@Temperature 90.0 °C
 >= 100 %
@Temperature 120 °C
 >= 100 %
@Temperature 150 °C
Elongation at Yield 3.0 %
Tensile Modulus 700 MPa
@Temperature 150 °C
 900 MPa
@Temperature 120 °C
 1200 MPa
@Temperature 90.0 °C
 2000 MPa
@Temperature 60.0 °C
 4200 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 55.0 kJ/m²
Charpy Impact, Notched 3.00 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 600 VA solution
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
Vicat Softening Point 240 °C
@Load 5.00 kg
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 1.50 mm
Oxygen Index 30 %
Glow Wire Test 960 °C
@Thickness 1.00 mm
GWFI/GWT
 960 °C
@Thickness 2.00 mm
GWFI/GWT
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 - 290 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chase Plastics CP Pryme® NN133GTL (DAM) Nylon 66, 33% Glass Fiber Reinforced, Toughened, Internally Lubricated
PTS Trimid® N66-G33L 33% Glass Fiber Reinforced Lubed Nylon 6/6
Akro-Plastic Akromid® A3 GF 35 black (2429) PA 6.6 Dry, 35% Glass Filled
A. Schulman ComAlloy Lubrilon® 62S1 Internally Lubricated, Nylon 6/6
PTS Trimid® N66-G33HL 33% Glass Fiber Reinforced Heat Stabilized, Lubed Nylon 6/6

PLATH9732 / 177428

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.