MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Borealis NAV107 LDPE, post-consumer recycled
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: NAV107 is a black low density polyethylene post-consumer recycled (rLDPE) supplied in pellet form for blown film applications. NAV107 is ideal LDPE used where sustainability and circularity matter. NAV107 is a post-consumer recycled including a large part of recycled post-consumer plastic waste coming from pre-sorted municipal (household) waste. NAV107 is part of the EuCertPlast certificate according to the European Standard EN 15343:2007 (certificate available upon request). Due to the nature of recycleds, some variation in color can be observed between batches. Cas No. 9002-88-4

Typical characteristics:

  • Black (includes black color masterbatch)
  • Available in homogenized 24-ton truckloads
  • Filtration: 100 µm
Applications:
  • Black garbage bags
  • Construction films
  • Black industrial films

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.510 g/cc0.0184 lb/in³ISO 60
Density 0.945 g/cc0.0341 lb/in³ISO 1183
Melt Flow 0.700 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.700 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133-1
Storage Temperature <= 50.0 °C<= 122 °F
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 150 %150 %527-3
Film Elongation at Break, TD 510 %510 %527-3
Tensile Modulus 0.250 GPa36.3 ksiMD; ISO 527-3
 0.290 GPa42.1 ksiTD; ISO 527-3
Elmendorf Tear Strength MD 122 g122 gISO 6383-2
Elmendorf Tear Strength TD 561 g561 gISO 6383-2
Dart Drop Test 35.0 g0.0772 lbISO 7765-1
Film Tensile Strength at Break, MD 12.0 MPa1740 psi527-3
Film Tensile Strength at Break, TD 12.0 MPa1740 psi527-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 160 - 190 °C320 - 374 °F
Moisture Content <= 0.0600 %<= 0.0600 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBORE9834 / 323191

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.