MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ganpati Exim 1400dtex/2 (1260D/2) Nylon-6 dipped tire cord
Categories: Other Engineering Material

Material Notes: The Nylon-6 dipped tire cord is a high and new technology product. It has such advantages as follows:
  • High breaking strength
  • Excellent impact resistance
  • High fatigue-proof strength
  • Good adhesive strength with rubber
  • Its is the high quality framework material of all kinds of rubber tire.

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 200.9 MPa>= 29140 psiQualified product
 >= 205.8 MPa>= 29850 psiFirst quality
 >= 215.6 MPa>= 31270 psiBest quality
Elongation at Break  9.0 - 10 %
@Load 6.79 kg
9.0 - 10 %
@Load 15.0 lb
Best quality
 8.7 - 10.3 %
@Load 6.79 kg
8.7 - 10.3 %
@Load 15.0 lb
First quality
 8.5 - 10.5 %
@Load 6.79 kg
8.5 - 10.5 %
@Load 15.0 lb
Qualified product
 
Thermal PropertiesMetricEnglishComments
Shrinkage  <= 6.0 %
@Temperature 150 °C,
Time 1800 sec
<= 6.0 %
@Temperature 302 °F,
Time 0.500 hour
Best quality, in Hot Air
 <= 6.5 %
@Temperature 150 °C,
Time 1800 sec
<= 6.5 %
@Temperature 302 °F,
Time 0.500 hour
First quality, in Hot Air
 <= 7.5 %
@Temperature 150 °C,
Time 1800 sec
<= 7.5 %
@Temperature 302 °F,
Time 0.500 hour
Qualified product, in Hot Air
 
Descriptive Properties
Adhesion by H-Test>127.4 N/cmQualified product
 >137.2 N/cmFirst quality
 >147 N/cmBest quality
Cord Gauge0.6-0.7 mmQualified product
 0.61-0.69 mmFirst quality
 0.62-0.68 mmBest quality
Resin Pick up3.5-5.5%Best quality
 3.5-5.5%First quality
 3.5-5.5%Qualified product
S-Twist35.5-38.5 T/10cmBest quality
 35.5-38.5 T/10cmFirst quality
 35.5-38.5 T/10cmQualified product
Variation of Elongation<6.3%Best quality
 <7.5%First quality
 <8.8%Qualified product
Variation of Tensile<3.8%Best quality
 <5.0%First quality
 <6.3%Qualified product
Water Ratio<1.0%Best quality
 <1.0%First quality
 <1.0%Qualified product
Z-Twist35.5-38.5 T/10cmBest quality
 35.5-38.5 T/10cmFirst quality
 35.5-38.5 T/10cmQualified product

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGANPATI014 / 317298

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.