MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Tra-Con Tra-Bond 216D02 Thixotropic No-Sag Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 216D02 is a thixotropic, two part epoxy adhesive formulated specifically for applications where a nonsagging adhesive is required. TRA-BOND 216D02 works in concert with TRA-CAST 3135 to perform `dam` and `fill` functions. This solvent free compound is readily mixed, handled and cured at room temperature to develop strong bonds to substrates including metals, ceramics, glass, wood and many plastics. Fully cured TRA-BOND 216D02 provides electrical insulation and superior resistance to water, petroleum product, gasoline, alcohol, salts, mild acids and alkalis.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 59600 cP
@Temperature 25.0 °C
59600 cP
@Temperature 77.0 °F
Mixed (sp #7, 10 rpm)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 84842 hrs @ 65°C
Adhesive Bond Strength 13.1 MPa1900 psiLap shear, alum to alum, 2 hrs @ 65°C
 
Thermal PropertiesMetricEnglishComments
CTE, linear 64.3 µm/m-°C35.7 µin/in-°FBelow Tg
 185 µm/m-°C103 µin/in-°FAbove Tg
Glass Transition Temp, Tg 70.0 °C158 °FUltimate Tg
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 240 min
@Temperature 65.0 °C
2.00 - 4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 80 min80 min
 
Descriptive Properties
Color Black
Thixotropic Index 4.41 rpm/10 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRAC047 / 70975

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.