MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Albis Plastics Polypropylene PP 14A12 CaCO3 30 , 30% Calcium Carbonate (CaCO3)  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Calcium Carbonate (CaCO3) Filler

Material Notes: Semi-crystalline Polypropylene Copolymer (PPCP)

Characteristics: Anti-Static: High Stiffness

Applications: Appliances, Furniture, Cases, Packaging and Novelties

Processing: Injection Molding (Melt Temperature: 430-535°F, Mold Temperature: 70-140°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ASTM D792
Melt Flow 12 g/10 min12 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.8 MPa3600 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Flexural Modulus 2.34 GPa339 ksiASTM D790
Izod Impact, Notched 0.530 J/cm0.993 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C160 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 221 - 279 °C430 - 534 °FInjection
Mold Temperature 21.0 - 60.0 °C69.8 - 140 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plastics Group Polifil® C-30 30% Calcium Carbonate-Reinforced Polypropylene
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Entec Hypro™ F PPH-CC30 Natural Homopolymer Polypropylene, 30% Calcium Carbonate Filled
Entec Hypro™ F PPC-CC30 Natural Copolymer Polypropylene, 30% Calcium Carbonate Filled
Albis Plastics Polypropylene PP 14A12 KR 30 , 30% Calcium Carbonate (CaCO3)

PZA1B83 / 21770

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.