MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Apcotex Apcoflex® NVC573E NBR/PVC Rubber Polyblend
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Apcoflex® NVC573E is a 70:30 Polyblend of Apcoflex medium NBR with PVC. . It contains non-staining stabilizer and comes in light tan coloured sheet form.

Applications: Apcoflex® NVC573E a Polyblend of Nitrile Rubber and PVC, combines the oil, fuel, thermal & abrasion resistance of NBR with ozone and weather resistance of PVC. Thus it is recommended for the manufacture of extruded and molded products suitable for out-door applications in automotive and industrial rubber goods. .NVC573E grade is highly suitable for the manufacture of LPG tubings and Fuel hoses, Profiles, Cable jackets, Bellows, Window seals, Grommets, conveyor belts etc.

CAS No: 9003-18-3 : NBR/ 9002-86-2 : PVC

Information provided by Apcotex Industries Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.70 %
Mooney Viscosity 55 - 65
@Temperature 100 °C
ML 1+4
Ash <= 1.0 %
Storage Temperature <= 35.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life <= 24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAPCOT015 / 315594

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.