MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chesterton ARC MXHT High temperature severe wear compound  (discontinued **)
Categories: Ceramic; Polymer; Thermoset; Epoxy

Material Notes: Description: An advanced ceramic composite for the protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack at elevated temperatures. It is applied at a thickness of 6mm (1/4”) or more. It is a 100% solids, non-shrinking coating. ARC MXHT is formulated with a high concentration of ceramic breads and fine ceramic particles for extremely abrasive environments where superior protection is needed. ARC MXHT is applied to a primed surface by trowel. It is chosen over ARC MX1 when abrasion resistance at elevated temperature is required.

Benefits:

  • Outlasts other wear resistant materials and coatings by 5-7 times
  • Excellent wear characteristics extend equipment’s operating cycles
  • Outperforms weld overlay or ceramic tiles
  • Tough resin structure resists thermal-mechanical shock.
  • Use in pH range 2-14 up to 130°C/266°F (wet service) and 230°C/466°F (dry service)
  • No need to post cure

Suggested Uses:Pumps

  • Elevated Temperature Fans/Blowers/Cyclones
  • Hoppers and Silos
  • Kiln Exhausters
  • Boiler Slag Systems
  • Electrostatic Precipitators

    Information provided by Chesterton

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 2.90 g/cc0.105 lb/in³Cured
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore D 8989ASTM D2240
    Tensile Strength at Break 29.6 MPa4300 psiASTM D638
    Elongation at Break 0.10 %0.10 %ASTM D638
    Flexural Strength 55.8 MPa8100 psiASTM D790
    Flexural Modulus 4.83 GPa701 ksiASTM D790
    Compressive Strength 162 MPa23500 psiASTM D695
    Adhesive Bond Strength >= 13.8 MPa>= 2000 psiASTM D4541
    Impact Test 13.6 J10.0 ft-lbReverse; ASTM D2794
     
    Thermal PropertiesMetricEnglishComments
    Maximum Service Temperature, Air 130 °C266 °FWet Service
     230 °C446 °FDry Service
     
    Processing PropertiesMetricEnglishComments
    Cure Time  360 min
    @Temperature 32.0 °C
    6.00 hour
    @Temperature 89.6 °F
    Light Load
     540 min
    @Temperature 25.0 °C
    9.00 hour
    @Temperature 77.0 °F
    Light Load
     1080 min
    @Temperature 16.0 °C
    18.0 hour
    @Temperature 60.8 °F
    Light Load
     4320 min
    @Temperature 32.0 °C
    72.0 hour
    @Temperature 89.6 °F
    Full Mechanical/Chemical
     5760 min
    @Temperature 25.0 °C
    96.0 hour
    @Temperature 77.0 °F
    Full Mechanical/Chemical
     10100 min
    @Temperature 16.0 °C
    168 hour
    @Temperature 60.8 °F
    Full Mechanical/Chemical
    Tack-Free Time  180 min
    @Temperature 32.0 °C
    3.00 hour
    @Temperature 89.6 °F
     240 min
    @Temperature 25.0 °C
    4.00 hour
    @Temperature 77.0 °F
     480 min
    @Temperature 16.0 °C
    8.00 hour
    @Temperature 60.8 °F
     
    Descriptive Properties
    ColorBlack

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    PPTCHS030 / 138142

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.