MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil AP60-007 High Density Polyethylene Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: AP60-007 is a medium molecular weight distribution high density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appearance and rigidity. AP60-007 offers the maximum in barrier properties available in high density polyethylene, and imparts minimum odor and taste to the packaged product.

Availability: Latin America, North America and South America

Additive:

  • Thermal Stabilizer: Yes
  • Antistatic: No
Applications:
  • Food packaging
  • Liquid Food Containers for Milk, Water and Juices
  • Thermoformed Parts

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.963 g/cc0.0348 lb/in³ASTM D4883
ESCR 100% Igepal® 10 hour10 hourASTM D1963
Melt Flow 0.73 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.73 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 31.7 MPa4600 psiASTM D638
Elongation at Break 350 %350 %ASTM D638
Flexural Modulus 1.72 GPa250 ksiASTM D790
Tensile Impact Strength 126 kJ/m²60.0 ft-lb/in²ASTM D1822
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 127 °C261 °FASTM D1525
Brittleness Temperature <= -76.1 °C<= -105 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil AA48-002 High Density Polyethylene Resin
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Petromont 8001 High Density Polyethylene Resin
Braskem BU004 Blow Molding High Density Polyethylene
Borealis BL2631 High Density Polyethylene

PEX99329 / 175565

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.