MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Eurofoam Porocell POR 304 B--175 EPDM Foam
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; gaskets.

Information provided by Eurofoam s.r.l.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.150 - 0.200 g/cc
Water Absorption <= 5.0 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 45 - 55
Elongation at Break >= 300 %
Compressive Yield Strength 0.0420 MPa
@Strain 25 %
 0.100 MPa
@Strain 50 %
Tear Strength 1.00 kN/m
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
Minimum Service Temperature, Air -40.0 °C
 
Descriptive Properties
Cellular StructureClosed
ColorBlack
Fire ResistanceFMVSS 302
VulcanizationSulfur

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rubatex R495 EPDM Rubber Foam Sheet
Rubatex R497 EPDM Rubber Foam Sheet
P & P Technology EPDM Closed Cell Sponge
Monmouth Rubber & Plastics Durafoam™ PMR 150 EPDM
Monmouth Rubber & Plastics Durafoam™ P291HD EPDM

PEUROF944 / 198174

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.