MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Eastalloy DA510 Polymer
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/PET Polyester Blend; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Eastalloy™ Polymer DA510 is a clear copolyester/polycarbonate alloy. This product has good impact strength, chemical resistance, heat resistance, dimensional stability, and low mold shrinkage.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Water Absorption 0.15 %0.15 %24h Immersion; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 56.0 MPa8120 psiASTM D638
Tensile Strength, Yield 50.0 MPa7250 psiASTM D638
Elongation at Break 195 %195 %ASTM D638
Elongation at Yield 5.5 %5.5 %ASTM D638
Flexural Strength 76.0 MPa11000 psiASTM D790
Flexural Modulus 2.10 GPa305 ksiASTM D790
Izod Impact, Notched  0.910 J/cm
@Temperature -40.0 °C
1.70 ft-lb/in
@Temperature -40.0 °F
ASTM D256
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NBNBASTM D4812
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ASTM D4812
Puncture Energy 55.0 J40.6 ft-lbPuncture Resistance @Max Load, 23°C; ASTM D3763
 49.0 J
@Temperature -40.0 °C
36.1 ft-lb
@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C171 °FASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 0.50 %0.50 %ASTM D1003
Transmission, Visible 86 %86 %Total Transmittance; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 266 - 288 °C511 - 550 °F
Mold Temperature 27.0 - 60.0 °C80.6 - 140 °F
Drying Temperature 88.0 °C190 °F
Dry Time 4 - 6 hour4 - 6 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aclo Acculoy POL063L Polycarbonate PET Alloy
Eastman Eastar GN071 Natural PETG Copolyester
Eastman DuraStar DS1000 Polymer, Natural
Toyobo VYLOPET® EMC407 Non-Reinforced
Wellman Wellpet® PR109-N1 Unfilled PET

PE9017 / 35073

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.