MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

Johnson Matthey Easy-flo™ 100 Flux Paste Brazing Flux
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: Easy-flo™ 100 Flux Paste is a brazing flux suitable for use with silver brazing filler metals and has a working range of 550-800°C. It is a smooth paste combining low melt viscosity with good resistance to overheating. Easy-flo™ 100 Flux Paste also sold as Mattiflux™ 100 Flux Paste.

Easy-flo™ 100 Flux Paste is suitable for use with silver brazing filler metals melting below 750°C (such as several of the Silver-flo™, Easy-flo™ and Argo-braze™ alloys). It is suitable for use on all the common engineering materials (copper, brass, mild steel and stainless steel), but not aluminum. Easy-flo™ 100 Flux Paste performs well on steels and stainless steels where its good overheat resistance is an advantage.

JM special purpose fluxes are required when brazing aluminum bronze, certain grades of stainless steel, tungsten, molybdenum and tungsten carbide or where protracted heating is involved.

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 550 - 800 °C1020 - 1470 °F
Solidus 550 °C1020 °F
Liquidus 800 °C1470 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Thermal Ceramics Cease 2000 Fire
Corning Gorilla® Glass 6 Display Glass

NJMMJ9728 / 186129

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.