MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
TSE Industries Millathane® 55 Millable Polyether Polyurethane Rubber, Typical 83A Compound
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Millathane® 55 is a high performance polyether millable urethane rubber which has been developed primarily for applications requiring low Mooney viscosity, high hardness sulfur-cured compounds such as rubber-covered rollers and molded products. Compounds have excellent abrasion resistance, high resilience (rebound), excellent ozone resistance, moderate oil and fuel resistance, and very good hydrolytic stability.

Information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 83
Tensile Strength 29.3 MPa
Elongation at Break 485 %
100% Modulus 0.695 ksi
@Strain 100 %
300% Modulus 2.41 ksi
@Strain 300 %
Resilience 43% Bashore
Tear Strength 47.4 kN/mDie C
 77.0 kN/mDie B
Abrasion 57mms loss; DIN Abrasion
 
Processing PropertiesOriginal ValueComments
Cure Time 11.0 min
@Temperature 160 °C
Press Cure, as Tested
 
Descriptive Properties
Formulation as Tested0.5Zinc Stearate
 1Silquest A-189
 1Struktol WB222
 1Thanecure® ZM
 100Millathane® 55
 13DBEEA (TP-95)
 2Carbowax 3350
 2MBT
 2AC 617A Polyethylene
 2.5RMS-80 (80% sulfur dispersion)
 4MBTS
 45Ultrasil VN3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber
Miracll M90 Thermoplastic Polyurethane (TPUR), Polyether Grade
Lubrizol ESTANE® 58215 Ether Based Thermoplastic Polyurethane
Kolon ELLAS K-395A Ether Based Thermoplastic Polyurethane

PMILL9941 / 223020

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.