Description: TECHNYL C 218L V30 is a polyamide 6 reinforced with 30% glass fiber and UV stabilized for injection molding. This product is available in black and grey colors. Key Properties: Excellent surface aspect; Dimensional stability; UV stabilized Benefits: This grade offers an excellent superficial aspect and excellent dimensional stability. It has good thermal and impact resistance. Applications: It is used in all sector of industry mainly in automotive industry as : external rear mirror support, external door handle; interior trims & switches. DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe. |