MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil 80 Exxon Aviation Oil EE Series
Categories: Fluid; Lubricant

Material Notes: Aviation Oil EE is the brand name of a premium quality line of ashless-dispersant piston engine oils. Formulated with select, highly refined base oils together with ashless-dispersant and anti-oxidant additives, Aviation Oil EE is designed to satisfy the requirements of all major engine manufacturers under all climatic conditions. To meet a wide range of requirements, Aviation Oil EE is available as monogrades in four viscosity grades: 65, 80, 100, and 120.

Aviation Oil EE oils are designed to meet the requirements of modern aircraft piston engines used in commercial, military and private aircraft. Ashless-dispersant aviation engine oils have attained wide-spread use due to their ability to keep engines cleaner than non-dispersant oils. The four grades of Aviation Oil EE meet the requirements of major engine manufacturers where monograde ashless-dispersant engine oils are recommended. Aviation Oil EE products are U.S. Military approved under SAE J1899, which replaced MIL-L-22851D and are listed in the U.S. Military Qualified Products List QPL-1899. Specific viscosity grades are approved by Pratt and Whitney, Teledyne Continental Motors, and Textron Lycoming and included in their respective Qualified Products Lists. Appropriate viscosity grades are recommended for Curtis-Wright, Franklin, and Rolls-Royce engines. Compatibility: Aviation Oil EE Series is compatible with nondispersant mineral oils as well as with other ashless-dispersant oils that meet the requirements of MIL-L-22851D/SAE J1899. They can be used in high-time engines that have previously used a straight mineral oil. If this is done, however, it is advisable to carry out the oil-screen inspection recommended by the engine manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.885 g/cc
@Temperature 15.6 °C
0.0320 lb/in³
@Temperature 60.1 °F
ASTM D4052
API Gravity 28.1 °28.1 °
Viscosity Measurement 120120Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 130 cSt130 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15.2 cSt15.2 cStASTM D445
Ash 0.00 %0.00 %SAE J1747
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 0.0100.010mgKOH/g; ASTM D664
 
Thermal PropertiesMetricEnglishComments
Pour Point -30.0 °C-22.0 °FASTM D97
Flash Point 253 °C487 °FASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WEXXON355 / 75780

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.