MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-SEAL S6305 Conductive Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.

Molded and Extruded.

RoHS Compliant

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.75 - 2.25 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55 - 75ASTM D2240
Tensile Strength at Break >= 200 psiASTM D412
Tensile Strength 203 psiTest 2; ASTM D412
 172 psi
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Vinyl Protectant; ASTM D412
 175 psi
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Tire Cleaner; ASTM D412
 178 psi
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to ClearVue®; ASTM D412
 197 psi
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Formula 409®; ASTM D412
 199 psi
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Cola; ASTM D412
 199 psi
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Tap Water; ASTM D412
 202 psi
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Windex®; ASTM D412
 207 psi
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Carpet Cleaner; ASTM D412
 207 psi
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Hairspray; ASTM D412
 207 psi
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Windshield Washer Solvent; ASTM D412
 211 psi
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Coffee; ASTM D412
Elongation at Break >= 100 %ASTM D412
 289 %Test 1; ASTM D412
 414 %Test 2; ASTM D412
 166 %
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Windex®; ASTM D412
 219 %
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Formula 409®; ASTM D412
 317 %
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to ClearVue®; ASTM D412
 326 %
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Hairspray; ASTM D412
 418 %
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Tire Cleaner; ASTM D412
 418 %
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Windshield Washer Solvent; ASTM D412
 433 %
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Vinyl Protectant; ASTM D412
 433 %
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Cola; ASTM D412
 439 %
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Coffee; ASTM D412
 439 %
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Tap Water; ASTM D412
 443 %
@Temperature 22.0 °C,
Time 252000 sec
50% RH, Exposure to Carpet Cleaner; ASTM D412
Tear Strength 8.75 kN/mASTM D624
Compression Set <= 30 %
@Temperature 100 °C,
Time 252000 sec
ASTM D395 Method B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.10 ohm-cmas supplied without pressure sensitive adhesive; CEPS-0002
Shielding Effectiveness >= 75 dB
@Frequency 4.00e+10 Hz
E Field; CHO-TM-TP08
 >= 100 dB
@Frequency 1e+8 Hz
E Field; CHO-TM-TP08
 >= 100 dB
@Frequency 5.00e+8 Hz
Plane Wave; CHO-TM-TP08
 >= 100 dB
@Frequency 2.00e+9 Hz
Plane Wave; CHO-TM-TP08
 >= 100 dB
@Frequency 1e+10 Hz
Plane Wave; CHO-TM-TP08
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.800 W/m-K
@Pressure 2.07 MPa
ASTM D5470
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -45.0 °CFlex TR10; ASTM D1329
Flammability, UL94 HB
 
Descriptive Properties
BinderSilicone
FillerNi/C
Heat Aging <0.25 ohm-cm125°C for 48 hrs; CEPS-0002

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics CHO-SEAL S6304 Conductive Elastomer
Parker Chomerics CHO-SEAL 1224 Conductive Elastomer
Parker Chomerics CHO-SEAL 1273 Conductive Elastomer
Parker Chomerics CHO-SEAL 1350 Conductive Elastomer
Parker Chomerics CHO-SEAL 1212 Conductive Elastomer

PCHOME114 / 28336

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.