MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wellman PP A422-LG20 Polypropylene with 20% Long Glass Fiber
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 20% Glass Fiber Filler

Material Notes: Long Glass Fiber Reinforced PP (LFT) produced by a pultrusion process. The pellet length is 10-15mm. PRET LFT provides outstanding mechanical performance and dimensional stability. Other benefits include high impact resistance, heat resistance, low warpage, low odor, and low VOC.

Features: Combination of high level of stiffness, strength, and toughness, Weight reduction, Dimensional stability, Corrosion resistance, Heat resistance.

Applications: Instrument Panel, Front End Module, Door Panel, Mirror Bracket, Floor Console.

Information provided by Wellman Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Filler Content 20 %20 %Glass; ISO 3451
Linear Mold Shrinkage 0.0015 - 0.0035 cm/cm
@Treatment Temp. 23.0 °C,
Time 173000 sec
0.0015 - 0.0035 in/in
@Treatment Temp. 73.4 °F,
Time 48.0 hour
PRET
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 80.0 MPa11600 psi5mm/min; ISO 527
Elongation at Break >= 2.8 %>= 2.8 %5mm/min; ISO 527
Tensile Modulus 5.10 GPa740 ksi1 mm/min; ISO 527
Flexural Strength 120 MPa17400 psi2mm/min; ISO 178
Flexural Modulus 4.50 GPa653 ksi2mm/min; ISO 178
Charpy Impact Unnotched 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched  1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 2.00 J/cm²
@Temperature -40.0 °C
9.52 ft-lb/in²
@Temperature -40.0 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 158 °C316 °FISO 75
Flammability Test 30
@Thickness 3.00 mm
30
@Thickness 0.118 in
ISO 3795
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 210 - 230 °C410 - 446 °F
Middle Barrel Temperature 230 - 250 °C446 - 482 °F
Front Barrel Temperature 230 - 250 °C446 - 482 °F
Nozzle Temperature 230 - 250 °C446 - 482 °F
Melt Temperature 230 - 250 °C446 - 482 °F
Mold Temperature 40.0 - 70.0 °C104 - 158 °F
Drying Temperature 80.0 - 100 °C
@Time 7200 - 14400 sec
176 - 212 °F
@Time 2.00 - 4.00 hour
Moisture Content <= 0.20 %<= 0.20 %
Injection Pressure 40.0 - 110 MPa5800 - 16000 psi
Screw Speed 20 - 70 rpm20 - 70 rpm
 
Descriptive Properties
Back Pressureas low as possible
Injection Speedlow to medium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWEL00905 / 250027

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.