MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Excel Industries Phosphorus Trichloride
Categories: Fluid

Material Notes: CSA No: 7719-12-2

Phosphorus Trichloride is an important raw material for many of the Organo phosphorus pesticides, Dye intermediates and Fire retardant Plasticizers. It is manufactured from Yellow Phosphorus, the technology of which has been indigenously developed by Excel. Excel’s P PCl3 CI, is exported worldwide and is considered to be at par with the best in the world.

Applications: PCl3 is a highly reactive chemical and is used in diverse applications:

  • It is a raw material used in the preparation of Phosphorus oxychloride, Phosphorus pentachloride and Thio phosphoryl chloride.
  • The Phosphorus acid esters obtained from the reaction of PCl3 and Alcohols or Phenols are used as Plasticizers and Stabilizers for plastic materials.
  • It is used as chlorinating agent in various processes.
  • It is used in the preparation of Fatty Acid Chlorides
  • It is used in the manufacture of Organophosphorus pesticides.
  • It is used in the manufacture of intermediates for bulk drugs like D-phenyl glycine which is a raw material for Cephalexin & Amoxycillin
  • It is used as an intermediate for Veterinary products
  • It is used in the manufacture of Napthol Dyes/Blue-G

Information provided by Excel Industries Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.558 - 1.562 g/cc
@Temperature 27.0 °C
1.558 - 1.562 g/cc
@Temperature 80.6 °F
Molecular Weight 137.35 g/mol137.35 g/mol
 
Chemical PropertiesMetricEnglishComments
Critical Temperature 285.5 °C545.9 °F
 
Thermal PropertiesMetricEnglishComments
Boiling Point 75.0 - 76.0 °C167 - 169 °F
Distillation Temperature 74.5 - 76.0 °C166 - 169 °FNot less than 95% by volume
 
Descriptive Properties
Assay>99.5%
Color<5 ppmHazen
Free Phosphorus<5 ppm
Iron<5 ppm
Physical stateClear, colorless liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay ALKAMIDE® C 212 Surfactant
ZEON Nipol® 1001LG Nitrile Elastomer
Versalis Intol® 1783 Emulsion Styrene-Butadiene Rubber
Versalis Europrene® 1723 Emulsion Styrene-Butadiene Rubber
Synthos BUNA™ SB 1502 Schkopau Cold Polymerized Emulsion Styrene Butadiene Rubber (E-SBR)

PEXCEL001 / 183477

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.