MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Abatron AboCast 8503-9/AboCure 8503-9 5-Minute Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AboCast 8503-9/AboCure 8503-9 is a very-fast-hardening 2-component epoxy adhesive, casting, and patching compound. It is a neutral-buff colored, non-sag, mineral-filled putty to be applied with trowel or other bladed tool for patching, filling, bonding, and anchoring in structural and dielectric applications. It does not have the brittleness typical of conventional 5-minute epoxies. It also provides high resistance to weather, water, salt spray, alkalis, diluted acids, several fuels, solvents, and other chemicals. Unlike other epoxies, a thin layer of this compound does not need any longer to harden than a thick casting.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.70 %
@Time 86400 sec
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 14
@Time 601 sec
 39
@Time 1800 sec
 70
@Time 3600 sec
 78
@Time 86400 sec
Shear Strength 1950 psiTensile lap
 
Processing PropertiesOriginal ValueComments
Pot Life 5.0 min
Gel Time 5.00 min
@Thickness 1.27 mm
 
Descriptive Properties
ColorTan
Parts by Weight (pbw)100AboCast 8503-9
 100AboCure 8503-9
ViscosityPutty

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PABC806 / 107790

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.