MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Toray PMC CFRT® TL-6000, 4 Layer Thermoplastic Composite Laminate
Categories: Polymer; Thermoplastic

Material Notes: Toray PMC CFRT® (TL-6000) is a reinforced thermoplastic composite that blends the benefits of a thermoplastic polymer matrix with woven carbon fibers for enhanced performance. Within the product range, 2 layer (MOD1, 2L), 3 layer (3L), or 4 layer (4L) products are available, all ultra-thin, lightweight, and resilient. This material can be drilled, ground, polished and adjusted after being formed with a heated gun. TL-6000 has a smooth high-gloss finish and transparent surface to show woven carbon fiber.

Features:

  • High strength and stiffness
  • High mechanical properties of “Thin & Light” (TL) laminates
  • Carbon fiber weave shown with a high-gloss and smooth finish
  • Choice of 2, 3, or 4 multilayers available
  • Core option available as MOD1 or with 4L
Product Type And Composition: CFRT® (Continuous Fiber Reinforced Thermoplastic) composite with carbon fiber and modified Polymethylmethacrylate (acrylic) resin

Typical Applications:

  • Orthosis knee and ankle bracing

Information provided by Toray Performance Materials Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³
Thickness 3430 - 3710 microns135 - 146 mil
 5080 - 5490 microns200 - 216 milwith 0.05” core
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength  245 MPa
@Thickness 3.42 mm
35500 psi
@Thickness 0.135 in
with 0.05” core
 365 MPa
@Thickness 3.42 mm
52900 psi
@Thickness 0.135 in
Flexural Modulus  28.4 GPa
@Thickness 3.42 mm
4120 ksi
@Thickness 0.135 in
 28.6 GPa
@Thickness 3.42 mm
4150 ksi
@Thickness 0.135 in
with 0.05” core
 
Descriptive Properties
Flexural Rigidity32250 N-cm3.42 mm, with 0.05” core
 9935 N-cm3.42 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTORAY8072 / 265470

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.