This product is a Lead free termination for single layer PZT ceramics. After firing the film has good adhesion and solderability. Screen Printing Equipment: semi-automatic, manual Screen Types: stainless steel, polyester, mesh 156-325 tpi Substrate: Polyimide, PET, PENInformation provided by Gwent Electronic Materials Ltd. |