MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Michelman® Michem® Prime 5931 Modified ethylene acrylic acid dispersion  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Description: Modified ethylene acrylic acid dispersion

Usage: Michem®Prime 5931 is a modified ethylene acrylic acid dispersion which provides improved adhesion to polyolefin substrates. It also exhibits excellent adhesion to paper, metallic and polymeric substrates as well as glass and polyester scrim. It can serve as a tie coat or primer and increases printability on metallic and polymeric substrates. It can be used as a heat sealable coating on most polymeric films, paper and foil. Patents Pending.

Application Data: Michem®Prime 5931 can be applied by flexographic or rotogravure coating methods. A typical application rate of 1-2 gsm dry coating weight is recommended for most heat seal applications. As a tie coat or print primer application rates of 0.2 to 0.5gsm are usually sufficient.

Food Contact Information when manufactured in the USA and Belgium:
FDA:
175.105: Components of adhesives(Restricted)
175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted)
176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)
176.180: Components of paper and paperboard in contact with dry foods. (Restricted)

Food Contact Information when manufactured in Singapore:
FDA:
175.105: Components of adhesives(Restricted)
175.300: Resinous and polymeric components of coatings. (Restricted)
175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted)
176.180: Components of paper and paperboard in contact with dry foods.

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.990 - 1.01 g/cc0.990 - 1.01 g/cc
Volatiles 71 - 72.5 %71 - 72.5 %
pH >= 7.0>= 7.0Recommended pH of system
 8.0 - 108.0 - 10
Brookfield Viscosity <= 100 cP<= 100 cPSpindle # 3, rpm 60
 
Descriptive Properties
AppearanceWhite translucent liquid
Emulsifier ChargeAmmoniated dispersion
Solids TypeProprietary

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Honeywell AClyn® 285P EAA copolymer
Honeywell AClyn® 246 EAA copolymer
BASF Lucalen® A 3120 M Ethylene/Acrylate Copolymer

WMICHEL163 / 135080

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.