MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker HDK® T40 Nutrition Silica
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Synthetic, hydrophilic amorphous silica, produced via flame hydrolysis.

Special features: White colloidal powder of high purity.

Application: HDK® T40NUTRITION shows the same product characteristics like HDK® N20, but in addition to the specified parameters of HDK® N20, the specification relevant for uses as Food and Feed Additive under E 551 according to Regulation (EU) 231/2012 are met. (Production according to ISO 9001, ISO 14001 and HACCP)

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.0400 g/cc0.00145 lb/in³tamped; DIN EN ISO 787-11
Density 2.20 g/cc0.0795 lb/in³DIN 51757
pH 3.8 - 4.33.8 - 4.34% dispersion; DIN EN ISO 787-9
Specific Surface Area 360 - 440 m²/g360 - 440 m²/gHydrophobic Silica
Evaporation Loss <= 1.5 %
@Temperature 105 °C,
Time 7200 sec
<= 1.5 %
@Temperature 221 °F,
Time 2.00 hour
DIN EN ISO 787-2
 
Component Elements PropertiesMetricEnglishComments
SiO2 >= 99.8 %>= 99.8 %based on the substance heated at 1000°C for 2 h; DIN EN ISO 3262-19
 
Descriptive Properties
Content<1 ppmMercury
 <250 ppmChloride (Cl)
 <3 ppmArsenic
 <5 ppmLead
 99-100.5%Silicone dioxide
Sieve residue<0.03%acc to Mocker >40 µm, DIN EN ISO 787-18

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker HDK® N20 Pharma Silica
Silicon, Si
Dicor Castable Fluormica Glass-Ceramic
Aremco Cerama-Fab™ 665
Aremco Ceramacast™ 646 Castable Ceramic

PWACK9356 / 204885

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.