MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Jackon JACKOCELL® S232 Expanded Polystyrene Packaging and Shape Molding
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: 100% Polystyrene.

Pre-expansion

This is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S232 which will lead the industry into the future. The unique design of polystyrene chains gives less sensitivity to steam - hence accurate density control over the unique property of S232. The combination of good properties is clearly a result of high technology in combination with extensive product development.

Shape Moulding

The unique design of polystyrene chains adds numerous advantages to Jackocell® S232 in high density shape molding. Fast molding cycles, good fusion, and easy to reach good surface. The additional broad molding window further reduces waste material and maintains a high quality to the extent that it can be recognized long term on productivity and financial earnings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0280 g/cc1.2 minute residence time pre-expander
 0.0380 g/cc2 minute residence time pre-expander
 0.0600 g/cc2.5 minute residence time pre-expander
 0.0900 g/cc2.7 minute residence time pre-expander
Bead Size 1.00 - 1.80 mm
 
Chemical PropertiesOriginal ValueComments
Blowing Agent Content <= 4.0 %Pentane
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 0.500 MPa30 g/l
 0.800 MPa50 g/l
 1.40 MPa70 g/l
 1.75 MPa90 g/l
Compressive Strength 2.55 MPa30 g/l
 4.08 MPa50 g/l
 6.63 MPa70 g/l
 9.38 MPa90 g/l
 
Descriptive Properties
Coefficient of Variation (%), max15
Molding Cycle Time (sec)23050 g/l, 24 hours @ 18°C
 40070 g/l, 24 hours @ 18°C
 45090 g/l, 24 hours @ 18°C
 7530 g/l, 24 hours @ 18°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam
Evonik ROHACELL® 100 WIND-F Polymethacrylimide Foam
Eurofoam Porocell POR 300/100 Ethylene Octane Metallocene EPDM Foam
Elliott Company ELFOAM® P600 Polyisocyanurate Foam
EconCore ThermHex THPP80-FN Polypropylene Honeycomb Core Sheet

PJACK004 / 85570

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.