MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker Vinnapas® 7220 E Vinyl Acetate-Ethylene Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product description: VINNAPAS® 7220 E is a semi flexible dispersible polymer powder based on vinyl esters, ethylene and acrylic acid ester for very good workability and excellent tensile adhesion strength after water immersion.

Properties: VINNAPAS® 7220 E is a polymer powder and is dispersible in water. VINNAPAS® 7220 E is ideal for modifying cementitious and gypsum-based mortars, e. g. tile adhesives. VINNAPAS® 7220 E contains a fine mineral filler as an antiblocking agent and is produced without the addition of organic solvents, plasticizers and film-forming agents.

Special features: VINNAPAS® 7220 E has no effect on rheological properties and is a polymer powder in the medium Tg range. It is suitable for formulating high-quality, low emissions flexible tile adhesive that feature excellent tensile adhesion strength, especially after immersion in water and exposure to freeze/thaw cycles.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.400 - 0.550 g/cc0.0145 - 0.0199 lb/in³DIN EN ISO 60
Solids Content >= 98 %>= 98 %DIN EN ISO 3251
Particle Size 400 µm400 µmmax 4% over; DIN EN ISO 4610
Ash <= 17.5 %<= 17.5 %
 
Descriptive Properties
Appearancewhite to light beige powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CHT Group EP QS EPI Engineered Polymers Quick Set Epoxy
A. Schulman BMC HT12-1023L Unsaturated Polyester Bulk Molding Compound
Overview of materials for Polyetheretherketone, PEEK, Aramid Fiber Filled
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled
Overview of materials for Polyamide-Imide, Molded

PWACK9617 / 205146

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.