MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Gabriel Versamid® G 2000 Amidoamine Resin
Categories: Polymer; Thermoset

Material Notes: Versamid® products have proven to be superior coatings resins in many applications, such as industrial maintenance and marine coatings, high-performance architectural paints and high-solids and conventional coatings.

Advantages:

  • Highly resistant to chemical and water corrosion
  • Strong adhesion to a variety of substrates
  • Long pot life
  • Lower sensitivity to substrate impurities
  • Most comply with FDA regulations
Principal Applications: Coatings, castings, potting, laminating, and adhesives

Comments/Advantages: Fast cure, good chemical resistance

Information provided by Gabriel Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.983 g/cc0.0355 lb/in³
Solids Content 100 %100 %Theo
Viscosity 1000 - 2500 cP1000 - 2500 cP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 70.3 MPa10200 psiAfter 7 days 25°C cure
Elongation at Break 5.0 %5.0 %After 7 days 25°C cure
Flexural Strength 122 MPa17700 psiAfter 7 days 25°C cure
Flexural Modulus 3.41 GPa495 ksiAfter 7 days 25°C cure
Compressive Strength 84.8 MPa12300 psiAfter 7 days 25°C cure
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg <= 92.0 °C<= 198 °F
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 8.0<= 8.0
 
Processing PropertiesMetricEnglishComments
Cure Time 270 min4.50 hourTack Free Time; 3 wet mils
 540 min9.00 hourThrough Cure; 3 wet mils
Pot Life 45.0 min45.0 min60% solids
Gel Time 38.0 min38.0 min200 mg Mass
 
Descriptive Properties
Amine Value580-620[mg KOH/g]
Chemical Resistance to 10% Acetic Acid15.44% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to 10% H4SO43.14% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to 10% HCl1.6% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to 10% NAOH0.43% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to Ethanol4.64% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to MEKDES% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical Resistance to Xylene4.94% weight gain after a 7 day 25°C cure followed by 21 days immersion at 25°C
Chemical TypeAmidoamine
PHR for Max DSC, Tg43190 EEW Epoxy
Theo Amine Hydrogen Equl Wt.82

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGABR990 / 230691

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.