MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lubrizol Estane® 91F65D EXP Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Type: Aliphatic polycaprolactone based Thermoplastic Polyurethane (TPU) with a 65 Shore D Hardness.

Features: Clear resin with excellent colour stability upon UV exposure.

Uses: Cast film extrusion, profile extrusion and molding.

Information provided by The 159 Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.111 g/cc1.111 g/ccISO 2781
Maximum Moisture Content 0.0200.020
Melt Flow 10 - 30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
10 - 30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 65
@Time 3.00 sec
65
@Time 0.000833 hour
ISO 868
Tensile Strength 34.0 - 37.0 MPa4930 - 5370 psiISO 527-2
Elongation at Break 250 - 300 %250 - 300 %ISO 527-2
100% Modulus 20.0 - 22.0 MPa
@Strain 100 %
2900 - 3190 psi
@Strain 100 %
ISO 527-2
300% Modulus 34.0 - 37.0 MPa
@Strain 300 %
4930 - 5370 psi
@Strain 300 %
ISO 527-2
 
Processing PropertiesMetricEnglishComments
Zone 1 170 - 180 °C338 - 356 °F
Zone 2 175 - 185 °C347 - 365 °F
Zone 3 180 - 190 °C356 - 374 °F
Zone 4 180 - 190 °C356 - 374 °F
Adapter Temperature 185 - 195 °C365 - 383 °F(5)
Die Temperature 180 - 190 °C356 - 374 °FZone 1 (6)
 180 - 190 °C356 - 374 °FZone 2
Drying Temperature 60.0 °C
@Time 14400 sec
140 °F
@Time 4.00 hour
Moisture Content <= 0.10 %<= 0.10 %
Dew Point -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR5018 / 238888

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.