MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Crystalbond™ 555 Washaway Mounting Adhesive & Accessory
Categories: Polymer; Adhesive

Material Notes: Low melting point of 120 ºF (49 ºC).

Typical Applications

  • Machining advanced ceramics
  • Lapping and polishing optical components
  • Dicing ceramic substrates
  • Dicing semiconductor wafers
  • Dicing ferrites, glasses and piezoelectrics
  • Dicing metal and optical single crystals
  • Mounting cross-sections for SEM
  • Backfilling components for support
  • Dry plasma etching

Vendors: Aremco’s Crystalbond and Wafer-Mount products are ideal for temporarily mounting ceramics, glass, quartz, and semiconductor substrates for dicing and polishing operations. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 220 cP
@Temperature 77.0 °C
#3 Spindle @6 RPM
 440 cP
@Temperature 63.0 °C
#3 Spindle @6 RPM
 1100 cP
@Temperature 46.0 °C
#3 Spindle @6 RPM
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 220 psi
 
Thermal PropertiesOriginal ValueComments
Melting Point 49.0 °CFlow Point
 
Descriptive Properties
Available FormsStick, 1/2” × 1” × 7”
ColorWhite
SolventHot Water
Weight0.15 Lbs/Stick

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAREM32 / 24296

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.